(a)Test procedure.
(1)Prepare 3 samples of cable each 2 feet long.
(2)Prior to testing, condition each test specimen for a minimum of 24 hours at a temperature of 70 ±10 °F (21.1 ±5.5 °C) and relative humidity of 55 ±10 percent. These environmental conditions shall be maintained during testing.
(3)Center the test specimen horizontally in the test chamber on the three rods. The three rods shall be positioned perpendicular to the longitudinal axis of the test specimen and at the same height, which permits the tip of the inner cone from the flame of the gas burner, when adjusted in accordance with the test procedure, to touch the test specimen. The specimen shall be maintained at this height for the duration of the flame test. The two outermost rods shall be placed so that 1 inch of cable extends beyond each rod. The third rod shall be placed at the midpoint of the cable. The specimen shall be free from external air currents during testing.
(4)Adjust the gas burner to give an overall blue flame 5 inches high with a 3-inch inner cone. There shall be no persistence of yellow coloration.
(5)Apply the tip of the inner cone from the flame of the gas burner for 30 seconds directly beneath the specimen centered between either and support and the center support.
(6)After subjecting the test specimen to external flame for the specified time, fully remove the flame of the gas from beneath the specimen without disturbing air currents within the test chamber.
(7)Record the amount of time the test specimen continues to burn after the flame from the gas burner has been removed. The duration of burning includes the burn time of any material that falls from the test specimen after the flame from the gas has been removed.
(8)Record the length of burned (charred) area of each test specimen measured longitudinally along the cable axis.
(9)Repeat the procedure for the remaining two specimens.
(b)Acceptable performance. Each of the three test specimens shall meet the following criteria:
(1)The duration of burning shall not exceed 60 seconds.
(2)The length of the burned (charred) area shall not exceed 6 inches.
★   the supreme law of the land   ★
Don't Tread on Me
E Pluribus Unum — out of many, one

"If you don't know your rights, you don't have any."

Marginalia · a citizen's law index
A research desk, not legal advice. Always read the cited source before relying on a summary.
Questions or an issue? support@self-law.org
disclaimerMarginalia is a research index, not a law firm. Nothing on this site is legal, tax, or financial advice and no attorney–client relationship is formed by using it. Statutes, regulations, and case law change; summaries, search results, AI output, and member posts may be incomplete, out of date, or wrong. Any interpretation drawn from material on this site should be validated by a licensed attorney in your jurisdiction before you act on it.