§ 1919.36. Heat treatment.

94 words·~1 min read·/us/cfr/t29/s§ 1919.36·

A research copy — for the controlling text, always check the official state or federal source. Not legal advice.

(a)The annealing of wrought iron gear required by this part shall be accomplished at a temperature between 1100° and 1200 °F. and the exposure shall be of between 30 and 60 minutes duration. After being annealed, the gear shall be allowed to cool slowly and shall then be carefully inspected. All annealing shall be carried out in a closed furnace.
(b)When heat treatment of loose gear made of other than wrought iron or steel is recommended by the manufacturer, it shall be carried out in accordance with the specifications of the manufacturer.
★   the supreme law of the land   ★
Don't Tread on Me
E Pluribus Unum — out of many, one

"If you don't know your rights, you don't have any."

Marginalia · a citizen's law index
A research desk, not legal advice. Always read the cited source before relying on a summary.
Questions or an issue? support@self-law.org
disclaimerMarginalia is a research index, not a law firm. Nothing on this site is legal, tax, or financial advice and no attorney–client relationship is formed by using it. Statutes, regulations, and case law change; summaries, search results, AI output, and member posts may be incomplete, out of date, or wrong. Any interpretation drawn from material on this site should be validated by a licensed attorney in your jurisdiction before you act on it.